Crystallinity,% | >90 | |||||||
PSD(D50),μm | ≤2.0 | |||||||
Surface Area(BET),㎡/g | >560 | |||||||
Pore Volume,ml/g | >0.3 | |||||||
Loss of lgnition(550℃,2hr),wt% | <5.0 | |||||||
SiO2,wt% | 7-11 | |||||||
Al2O3,wt% | 40-44 | |||||||
P2O5,wt% | 46-50 | |||||||
Packaging size | Net weight: 25Kg/40Kg per bag | |||||||
Package | The inner packing is PE bag,the out packing is Paper-plastic composite bag | |||||||
Storage | Bagged, dry sealed |